для размещения заказа - kennametal@kennametal.su Cutting Conditions
Speed vc (m/min)
Speed vc (m/min) Wear Resistance
For all Families -- +
Coolant Recommendation CVD CVD CVD Speed min. - max. PVD Uncoated Uncoated
Standard Standard Standard Micrograin Cermet Cermet
Recommended Possible Uncoated
Micrograin
ISO Materials Rm and MP91M SC6525 SC3025 GH1* SP1019 SA9808 SA9608
Hardness
Unalloyed 140 - 345 140 - 370 240 - 345 225 - 380 240 - 345 265 - 380
Steel <600 N/mm2
<180 HBN
P <950 N/mm2 120 - 305 120 - 325 215 - 305 200 - 335 215 - 305 235 - 335
<280 HBN
Alloyed 700-950 N/mm2 105 - 270 105 - 290 190 - 270 175 - 295 190 - 270 205 - 295
Steel 200-280 HBN
950-1200 N/mm2
Stainless 280-355 HBN 80 - 205 80 - 210 140 - 205 130 - 225 140 - 205 155 - 225
1200-1400 N/mm2
M Steel 355-415 HBN 50 - 130 50 - 140 90 - 130 85 - 145 90 - 130 100 - 145
PH Stainless Austenitic + Ferritic 215 -305 200 - 335 235 -335
300 series
K Cast Iron 195 - 275 180 - 305 Technical
Martensitic 215 - 305
N Aluminium 400 series
& Alloys 90 - 180 85 - 145 100 - 200
Refractory
P.H. 145 - 365 145 - 390 150 - 395 135 - 290 240 - 400 280 -400
115 - 285 115 - 305
Grey 120 - 335 120 - 245 185 - 340 220 -315
GG-Ft 105 - 260
105 - 275 115 - 200 170 - 285 200 -285
Spheroidal-Ductile
GGG-FGS 400 - 3050 400 - 2745
Malleable
GTS - MN/MP
295 - 2440 295 - 2135
Aluminium & Alloys
< 16% Si 116 HBN
Aluminium + Silicon
> 16% Si 92 HBN
Iron Based 40 - 67 50 - 75
High Cobalt Based 37 - 63 48 - 70
Nickel Based
S Temperature
Alloys 42 - 72 52 - 75
Titanium Based 61 - 103 60 - 95
H Hard Hard Steel 50 - 105 50 - 110
Materials >1400 N/mm2
>415 HBN 40 - 95 45 - 100
Chilled Cast Iron
>1400 N/mm2
> 400 HBN
* Note: Wiper Insert SPHX12M512EN GH1 can be used for Steel, Steel Alloys, Stainless Steel and Cast Iron.
* Note: All other GH1 Grade Inserts are only for Aluminium or Cast Iron depending on the selected Geometry.
www.kennametal.su A291