Recommended Speeds
Speed vc (m/min) Cartridge Face Mills
80.0VOD45-_R-06 -- Wear Resistance +
Series
Speed mi.n. - max..
Coolant Recommendation CVD PVD PVD CVD CVD Uncoated Uncoated
X Grade Standard Standard Standard Micrograin Cermet
Recommended Possible Standard
MP91M
ISO Materials Rm and X500 SP6519 SP4019 140 - 345 SC3025 GH1* SA9608
Hardness
Unalloyed <600 N/mm2 130 - 270 130 - 295 120 - 305 240 - 345 265 - 380
Steel <180 HBN 105 - 270
115 - 240 115 - 260
<950 N/mm2 215 - 305 235 - 335
<280 HBN 80 - 205
P 700-950 N/mm2 100 - 210 100 - 230 50 - 130 190 - 270 205 - 295
200-280 HBN
Alloyed 75 - 160 75 - 175 145 - 365
Steel 950-1200 N/mm2 115 - 285 140 - 205 155 - 225
280-355 HBN
105 - 260
1200-1400 N/mm2 50 - 100 50 - 110 90 - 130 100 - 145
355-415 HBN
M Stainless Austenitic + Ferritic 115 - 250 115 - 270 120 - 280 215 -305 235 -335
Steel 300 series 100 - 220 105 - 235 110 - 250
195 - 275 215 - 305
Martensitic
400 series
PH Stainless Refractory 50 - 110 50 - 120 50 - 130 90 - 180 100 - 200
P.H.
Grey 140 - 295 150 - 395 135 - 290 280 -400
GG-Ft
K Cast Iron Spheroidal-Ductile 110 - 240 120 - 335 120 - 245 220 -315
GGG-FGS
Malleable 100 - 220 105 - 275 115 - 200 200 -285
GTS - MN/MP
Aluminium & Alloys 400 - 3050
N Aluminium < 16% Si 116 HBN
& Alloys Aluminium + Silicon 295 - 2440
> 16% Si 92 HBN
Iron Based 23 - 48 23 - 55 24 - 63 50 - 75
High Cobalt Based 21 - 44 22 - 48 23 - 52 48 - 70
Nickel Based 24 - 51 25 - 55 26 - 59
S Temperature
Alloys 52 - 75
Titanium Based 35 - 73 36 - 79 37 - 84 60 - 95
H Hard Hard Steel 50 - 100
Materials >1400 N/mm2
>415 HBN 40 - 90
Chilled Cast Iron
>1400 N/mm2
> 400 HBN
* Note: ODET04..-441 in Grade GH1 can only be used for Aluminium.
* Note: SPHX12M512EN GH1 can be used for Steel, Steel Alloys, Stainless Steel, Cast Iron and High Temperature Alloys.